Temperature effects and superconductors

A motor winding that measures 12 Ω on the bench can be well above 14 Ω once it is running hot, and some materials lose every trace of resistance when cooled far enough. This topic shows how to predict resistance at any working temperature and what happens at the cold extreme.

Why temperature matters

Resistance values in tables are quoted at a reference temperature, usually 20 °C. Real conductors rarely stay there: windings warm up in use, outdoor lines freeze in winter, and lamp filaments glow at thousands of degrees. In a metal, a rise in temperature makes the lattice ions vibrate harder, so drifting electrons collide more often and resistance rises. Metals therefore have a positive temperature coefficient. Semiconductors, as "Semiconductors" explained, usually do the opposite: heat frees more carriers, so their resistance falls. Over ordinary working ranges, a metal's resistance changes almost linearly with temperature, which makes it easy to predict.

The inferred absolute temperature

Plot a metal's resistance against temperature and the curve is close to a straight line over the normal range. Extend that line downwards and it meets zero resistance at a temperature called the inferred absolute temperature, \(T_i\): about \(-234.5\) °C for copper, \(-236\) °C for aluminium and \(-204\) °C for tungsten. Real metals do not actually reach zero there; the line is just a convenient model. Because resistance is proportional to the distance from \(T_i\) along the line,

\frac{R_2}{R_1} = \frac{|T_i| + T_2}{|T_i| + T_1}

with \(T_1\) and \(T_2\) in °C. Use the magnitude of \(T_i\), so for copper the factors are \(234.5 + T\).

Worked example: a hot motor winding

A copper winding measures 12.0 Ω at 20 °C. What is its resistance when it runs at 85 °C? 1. Copper: \(|T_i| = 234.5\) °C. 2. Ratio:

\frac{R_2}{12.0} = \frac{234.5 + 85}{234.5 + 20} = \frac{319.5}{254.5}

3. Solve: \(R_2 = 12.0 \times 1.2554 = 15.1\) Ω. 4. Check the direction and size: the winding got hotter, so resistance must rise, and a 65 °C rise in copper gives about 0.39% per degree, roughly 25%. Engineers turn this round to estimate a winding's internal temperature by measuring its resistance hot and cold.

The temperature coefficient α

An equivalent form uses the temperature coefficient of resistance, \(\alpha\), the fractional change in resistance per degree at a stated reference temperature:

R = R_{20}[1 + \alpha_{20}(T - 20)]

For copper, \(\alpha_{20} = 0.00393\) per °C, which is just \(\frac{1}{234.5 + 20}\), so the two methods agree. Aluminium's is about 0.00391 per °C. Alloys such as nichrome have very small coefficients, near 0.0004 per °C, and constantan's is close to zero, which is why precision resistors and heating elements use alloys. A negative \(\alpha\) means resistance falls with temperature, as in most semiconductors.

Worked example: a line on a winter night

An aluminium overhead-line conductor has a resistance of 0.250 Ω at 20 °C. Find its resistance at \(-10\) °C. 1. Change in temperature: \(T - 20 = -10 - 20 = -30\) °C. 2. Apply the coefficient: \(R = 0.250[1 + 0.00391(-30)] = 0.250(0.8827)\). 3. Result: \(R = 0.221\) Ω. 4. Check with the inferred absolute temperature: \(0.250 \times \frac{236 - 10}{236 + 20} = 0.250 \times \frac{226}{256} = 0.221\) Ω, which agrees. Cold conductors have lower resistance, so the same current loses a little less energy in the line.

PPM ratings for resistors

Resistor data sheets state the temperature coefficient in parts per million per degree, ppm/°C. The change is

\Delta R = \frac{R \times \text{ppm} \times \Delta T}{10^{6}}

Carbon-film resistors are typically several hundred ppm/°C, metal-film parts around 50 to 100 ppm/°C, and precision foil resistors only a few. For example, a 10.0 kΩ metal-film resistor rated 50 ppm/°C, warmed from 25 °C to 70 °C, changes by \(\frac{10{,}000 \times 50 \times 45}{10^{6}} = 22.5\) Ω, or 0.225%. That is negligible in most circuits but matters in measurement equipment.

Temperature sensing and filaments

The predictable rise of metal resistance makes a good thermometer. A platinum resistance temperature detector, the Pt100, has 100 Ω at 0 °C and a coefficient of about 0.00385 per °C, so at 50 °C it reads about 119 Ω. Temperature has the opposite effect on usefulness in a lamp. A tungsten filament runs at well over 2000 °C, where its resistance is roughly ten times or more its cold value. At switch-on the cold filament therefore draws a large inrush current for a moment, which is why incandescent lamps often fail at the moment they are switched on.

Superconductivity

In 1911 Heike Kamerlingh Onnes found that mercury cooled to about 4.2 K, close to absolute zero, lost all measurable resistance. Below a material's critical temperature \(T_c\), a superconductor carries direct current with zero resistance, so a current set up in a superconducting loop can circulate for years. It also expels magnetic fields from its interior, the Meissner effect, found in 1933. In 1957 Bardeen, Cooper and Schrieffer explained conventional superconductivity: electrons bind into Cooper pairs that move through the lattice without scattering. Superconductivity disappears if the temperature, the magnetic field or the current density exceeds its critical value.

High-temperature superconductors

For decades \(T_c\) stayed below about 30 K, so cooling needed expensive liquid helium. In 1986 Georg Bednorz and Alex Müller found superconductivity at about 35 K in a copper-oxide ceramic, and in 1987 yttrium barium copper oxide (YBCO) was found to superconduct at about 92 K, above the 77 K boiling point of cheap liquid nitrogen. Copper-oxide materials reach about 133 K at normal pressure in their ordinary, stable form; hydrogen-rich compounds have gone higher, but only under enormous pressures. Uses include MRI scanner magnets, wound from niobium-titanium wire and cooled by liquid helium, particle-accelerator magnets, maglev trains, sensitive magnetometers and some power cables.

Common mistakes to avoid

First, assuming resistance is proportional to the Celsius temperature itself; it is proportional to \(|T_i| + T\). Second, putting the sign of \(T_i\) into the formula, as in \(-234.5 + T\). Third, using \(\alpha_{20}\) with a reference resistance measured at some other temperature. Fourth, forgetting that semiconductors and some alloys behave differently from pure metals. Fifth, thinking a superconductor has merely very low resistance; below \(T_c\) its dc resistance is zero. Sixth, assuming high-temperature superconductors work at room temperature: they still need deep cooling.

Key takeaways

Metal resistance rises almost linearly with temperature: R₂/R₁ = (|Tᵢ| + T₂)/(|Tᵢ| + T₁), with Tᵢ about −234.5 °C for copper and −236 °C for aluminium. Equivalently R = R₂₀[1 + α₂₀(T − 20)], with α₂₀ = 0.00393 per °C for copper. Resistor drift is rated in ppm/°C. Platinum sensors and filament inrush currents both follow from the effect. Superconductors have zero dc resistance below Tc and expel magnetic fields; YBCO (1987, about 92 K) works in liquid nitrogen, while MRI magnets use liquid-helium-cooled niobium-titanium.

Flashcards

Flashcard

Positive temperature coefficient

Resistance rises as temperature rises

Typical of metals.

Test your understanding

Question 1 of 5

A copper coil measures 20.0 Ω at 20 °C and is then warmed to 60 °C. Taking Tᵢ = −234.5 °C, what does it measure now?

Question 2 of 5

A 4.7 kΩ resistor is rated 100 ppm/°C. By how much does its resistance change when it warms by 30 °C?

Question 3 of 5

Which pair of properties describes a superconductor below its critical temperature?

Question 4 of 5

Why was the 1987 discovery that YBCO superconducts at about 92 K so important?

Question 5 of 5

What does the inferred absolute temperature of copper, −234.5 °C, represent?